Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA46 TE351 DSM HOLAND
Stanyl®
Electronic and electrical components,Casters
Flame retardant,Thermal stability
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | DSM HOLAND/TE351 |
---|---|---|---|
Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 160 °C |
Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 9.0E-5 cm/cm/°C |
Flow | ISO 11359-2 | 9.0E-5 cm/cm/°C | |
Melting temperature | ISO 11357-3 | 295 °C | |
RTI Elec | 0.75 mm | UL 746 | 65.0 °C |
mechanical properties | Test Condition | Test Method | DSM HOLAND/TE351 |
---|---|---|---|
Bending modulus | ISO 178 | 2500 Mpa | |
Nominal tensile fracture strain | ISO 527-2 | 20 % | |
Tensile modulus | ISO 527-2 | 3000 Mpa | |
tensile strength | Yield | ISO 527-2 | 60.0 Mpa |
Physical properties | Test Condition | Test Method | DSM HOLAND/TE351 |
---|---|---|---|
density | ISO 1183 | 1.37 g/cm³ | |
Shrinkage rate | 横向Flow | ISO 294-4 | 2.0 % |
Flow | ISO 294-4 | 2.0 % | |
Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 2.0 % |
impact performance | Test Condition | Test Method | DSM HOLAND/TE351 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.0 kJ/m² |
-30°C | ISO 179/1eA | 5.0 kJ/m² | |
Impact strength of cantilever beam gap | -40°C | ISO 180/1A | 5.0 kJ/m² |
23°C | ISO 180/1A | 8.0 kJ/m² | |
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 85 kJ/m² |
23°C | ISO 179/1eU | 85 kJ/m² |
flammability | Test Condition | Test Method | DSM HOLAND/TE351 |
---|---|---|---|
Flammability level | UL 94 | V-0 |