Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
POM KL-4030 BK SABIC INNOVATIVE US
LNP™ LUBRICOMP™ 
Plastic bag,Medical and nursing supplies
Low extract,wear resistant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodSABIC INNOVATIVE US/KL-4030 BK
Impact strength of cantilever beam gap23°CISO 180/1A3.0 kJ/m²
Suspended wall beam without notch impact strength23°CISO 180/1U46 kJ/m²
thermal performanceTest ConditionTest MethodSABIC INNOVATIVE US/KL-4030 BK
Heat Deflection Temperature0.45MPa,Unannealed,64.0mmSpanISO 75-2/Bf149 °C
0.45MPa,未退火,3.20mmASTM D648158 °C
1.8MPa,未退火,3.20mmASTM D64897.0 °C
1.8MPa,未退火,64.0mm跨距ISO 75-2/Af88.0 °C
Linear coefficient of thermal expansionTD:-30to30°CASTM D6961.1E-04 cm/cm/°C
MD:-30到30°CASTM D6961.1E-04 cm/cm/°C
mechanical propertiesTest ConditionTest MethodSABIC INNOVATIVE US/KL-4030 BK
bending strengthASTM D79075.8 Mpa
coefficient of frictionStaticASTM D3702Modified0.17
DynamicASTM D3702Modified0.35
elongation断裂ASTM D63819 %
屈服ASTM D63810 %
flexural modulus50.0mm跨距ASTM D7902210 Mpa
ISO 1782250 Mpa
Tensile modulusASTM D6382530 Mpa
ISO 527-2/12460 Mpa
Tensile strain断裂ISO 527-2/516 %
屈服ISO 527-2/59.0 %
tensile strength断裂ISO 527-2/546.0 Mpa
屈服ASTM D63848.0 Mpa
屈服ISO 527-2/546.0 Mpa
断裂ASTM D63848.0 Mpa
Wear factorRingASTM D3702Modified0.300 10^-10in^5-min/ft-lb-hr
WasherASTM D3702Modified11.0 10^-10in^5-min/ft-lb-hr
Physical propertiesTest ConditionTest MethodSABIC INNOVATIVE US/KL-4030 BK
shrinkage rateMD:24小时ASTM D9551.0-3.0 %
TD:24hrASTM D9551.0-3.0 %
Water absorption rate24hr,50%RHASTM D5700.20 %
平衡,23°C,50%RHISO 620.29 %