Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA46 OCD2305 DSM HOLAND
Stanyl®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | DSM HOLAND/OCD2305 |
|---|---|---|---|
| Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 275 °C |
| 1.8 MPa, Unannealed | ISO 75-2/A | 240 °C | |
| Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 9.0E-5 cm/cm/°C |
| Flow | ISO 11359-2 | 2.5E-5 cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 284 °C |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/OCD2305 |
|---|---|---|---|
| Bending modulus | ISO 178 | 9000 Mpa | |
| Tensile modulus | 200°C | ISO 527-2 | 2000 Mpa |
| -- | ISO 527-2 | 8500 Mpa | |
| Tensile strain | Break | ISO 527-2 | 3.3 % |
| Break, 200°C | ISO 527-2 | 20 % | |
| tensile strength | Break, 200°C | ISO 527-2 | 50.0 Mpa |
| Break | ISO 527-2 | 160 Mpa |