Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM TX-21 KEP KOREA
KEPITAL®
--
Medium viscosity,copolymer,wear resistant
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | KEP KOREA/TX-21 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 89.0 °C |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 1.3E-04 cm/cm/°C |
| Melting temperature | ISO 11357-3 | 165 °C |
| mechanical properties | Test Condition | Test Method | KEP KOREA/TX-21 |
|---|---|---|---|
| Bending modulus | ISO 178 | 2350 Mpa | |
| bending strength | ISO 178 | 79.0 Mpa | |
| Tensile modulus | ISO 527-2 | 2500 Mpa | |
| Tensile strain | Yield | ISO 527-2 | 10 % |
| Break | ISO 527-2 | 33 % | |
| tensile strength | ISO 527-2 | 58.0 Mpa |
| Electrical performance | Test Condition | Test Method | KEP KOREA/TX-21 |
|---|---|---|---|
| Surface resistivity | IEC 60093 | 1E+16 ohms | |
| Volume resistivity | IEC 60093 | 1E+14 ohms·cm |
| Physical properties | Test Condition | Test Method | KEP KOREA/TX-21 |
|---|---|---|---|
| density | ISO 1183 | 1.39 g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 16 g/10min |
| Shrinkage rate | MD:3.00mm | Internal Method | 2.0 % |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.20 % |
| impact performance | Test Condition | Test Method | KEP KOREA/TX-21 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 7.5 kJ/m² |
| -30°C | ISO 179/1eA | 5.0 kJ/m² |
| flammability | Test Condition | Test Method | KEP KOREA/TX-21 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |