Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM LT-805 ASAHI JAPAN
TENAC™
Industrial applications,Automotive Applications,bearing,Computer components,Engine parts,Mechanical/mechanical parts
High mobility,Medium viscosity
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Basic Performance | Test Condition | Test Method | ASAHI JAPAN/LT-805 |
|---|---|---|---|
| melt mass-flow rate | 190℃/2.16kg | ASTM D1238 | 22 g/10min |
| Water absorption rate | Saturation | ASTM D570 | 0.2 % |
| thermal performance | Test Condition | Test Method | ASAHI JAPAN/LT-805 |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,unannealed | ASTM D648 | 172 ℃ |
| Linear coefficient of thermal expansion | Flow | ASTM D696 | 0.0001 cm/cm/℃ |
| UL flame retardant rating | 0.76mm | UL 94 | HB |
| mechanical properties | Test Condition | Test Method | ASAHI JAPAN/LT-805 |
|---|---|---|---|
| Bending modulus | ASTM D790 | 2840 MPa | |
| bending strength | ASTM D790 | 93.2 MPa | |
| Impact strength of cantilever beam gap | ASTM D256 | 68.6 J/m | |
| tensile strength | ASTM D638 | 63.7 MPa |
| Electrical performance | Test Condition | Test Method | ASAHI JAPAN/LT-805 |
|---|---|---|---|
| Arc resistance | 3.12mm | ASTM D495 | 150 sec |
| Physical properties | Test Condition | Test Method | ASAHI JAPAN/LT-805 |
|---|---|---|---|
| Rockwell hardness | M-Scale | ASTM D785 | 92 |
| Shrinkage rate | Flow | ASTM D955 | 1.8-2.2 % |