Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 A3GF13 AKRO-PLASTIC GERMANY
AKROMID®
engineering application
Filler: Glass fiber reinf,13% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF13 |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 75 kJ/m² |
-30°C | ISO 179/1eU | 55 kJ/m² |
Supplementary Information | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF13 |
---|---|---|---|
ReinforcementContent | ISO 1172 | 13 % |
Mechanical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF13 |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 5200 Mpa | |
tensile strength | 断裂 | ISO 527-2/5 | 125 Mpa |
bending strength | ISO 178 | 180 Mpa | |
Flexural modulus | ISO 178 | 4800 Mpa | |
Tensile strain | 断裂 | ISO 527-2/5 | 4.0 % |
physical property | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF13 |
---|---|---|---|
Shrinkage rate | TD | ISO 294-4 | 0.90 % |
MD | ISO 294-4 | 0.30 % |
Thermal performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3GF13 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 261 °C |
melting temperature | DIN EN11357-1 | 260 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 244 °C |