PP AP3AW EXXONMOBIL SINGAPORE
ExxonMobil™ 
Battery box、Engine hood parts、Automotive sector、Application in the automo、Parts under the hood of a
Low warpage、High rigidity、High impact resistance、Middle flow、Light resistance
UL
TDS
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodEXXONMOBIL SINGAPORE/AP3AW
Charpy Notched Impact Strength23°CISO 179/1eA9.9 kJ/m²
-30°CISO 179/1eA3.3 kJ/m²
-20°CISO 179/1eA3.9 kJ/m²
Dart impact-29°C,3.18mmASTM D542018.1 J
Impact strength of cantilever beam gap23°CISO 180/1A8.8 kJ/m²
-40°CISO 180/1A3.4 kJ/m²
Charpy Notched Impact Strength0°CISO 179/1eA4.9 kJ/m²
Impact strength of cantilever beam gap-18°CASTM D256A35 J/m
23°CASTM D256A90 J/m
-18°CISO 180/1A4.5 kJ/m²
hardnessTest ConditionTest MethodEXXONMOBIL SINGAPORE/AP3AW
Rockwell hardnessASTM D78596
Mechanical propertiesTest ConditionTest MethodEXXONMOBIL SINGAPORE/AP3AW
Tensile modulusISO 527-2/11500 Mpa
tensile strength 屈服ISO 527-2/5025.7 Mpa
Flexural modulus1%正割5ASTM D790B1520 Mpa
tensile strength 屈服3ASTM D63827.1 Mpa
elongation屈服ISO 527-2/505.7 %
屈服3ASTM D6385.6 %
Flexural modulus--6ISO 1781340 Mpa
1%正割4ASTM D790A1340 Mpa
physical property Test ConditionTest MethodEXXONMOBIL SINGAPORE/AP3AW
melt mass-flow rate230°C/2.16kgASTM D123810 g/10min
Thermal performanceTest ConditionTest MethodEXXONMOBIL SINGAPORE/AP3AW
Heat distortion temperature0.45MPa,未退火,HDTASTM D64899.4 °C
1.8MPa,未退火,HDTISO 75-2/A53.4 °C
0.45MPa,退火,HDTASTM D648116 °C
0.45MPa,未退火,HDTISO 75-2/Bf92.5 °C