HDPE EX3 (GM 5010 T2N) Iran Amir Kabir
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | Iran Amir Kabir/EX3 (GM 5010 T2N) |
---|---|---|---|
Static pressure strength | 80oc,4N/mm2 | DIN 8074 &DIN 8075 &ISO 1167 | 1000min hours |
Mechanical properties | Test Condition | Test Method | Iran Amir Kabir/EX3 (GM 5010 T2N) |
---|---|---|---|
Impact strength of cantilever beam gap | ISO 179/1eA | >12 mj/mm2 |
physical property | Test Condition | Test Method | Iran Amir Kabir/EX3 (GM 5010 T2N) |
---|---|---|---|
density | ISO 1183 | 0.945±0.002 g/cm3 | |
melt mass-flow rate | 190℃/5kg | ISO 1133 | 0.45±0.05 g/cm |
FRR | 21.3/5 | 28±4 | |
melt mass-flow rate | 190℃/21.6kg | ISO 1133 | 12±3 g/cm |