Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP Homopolymer ADDILENE PMD 50408 ADDIPLAST FRANCE
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | ADDIPLAST FRANCE/ADDILENE PMD 50408 |
---|---|---|---|
Impact strength of cantilever beam gap | ISO 180/1A | 2.0 kJ/m² | |
Impact strength of simply supported beam without notch | ISO 179/1eU | 17 kJ/m² | |
Charpy Notched Impact Strength | ISO 179/1eA | 2.0 kJ/m² |
hardness | Test Condition | Test Method | ADDIPLAST FRANCE/ADDILENE PMD 50408 |
---|---|---|---|
Shore hardness | 邵氏D | ISO 868 | 76 |
Mechanical properties | Test Condition | Test Method | ADDIPLAST FRANCE/ADDILENE PMD 50408 |
---|---|---|---|
tensile strength | 断裂 | ISO 527-2 | 20.0 MPa |
Tensile strain | 断裂 | ISO 527-2 | 40 % |
tensile strength | 屈服 | ISO 527-2 | 24.0 MPa |
Flexural modulus | ISO 178 | 2000 MPa |
Electrical performance | Test Condition | Test Method | ADDIPLAST FRANCE/ADDILENE PMD 50408 |
---|---|---|---|
Compared to the Leakage Tracking Index (CTI) | 解决方案A | IEC 60112 | PLC 0 |
flammability | Test Condition | Test Method | ADDIPLAST FRANCE/ADDILENE PMD 50408 |
---|---|---|---|
Hot filament ignition temperature | IEC 60695-2-13 | 960 °C | |
UL flame retardant rating | 1.60mm | UL 94 | V-0 |
Limiting Oxygen Index | ISO 4589-2 | 40 % |
physical property | Test Condition | Test Method | ADDIPLAST FRANCE/ADDILENE PMD 50408 |
---|---|---|---|
density | ISO 1183/A | 0.990 g/cm³ | |
Melt volume flow rate | 230°C/2.16kg | ISO 1133 | 6.00 cm³/10min |
Thermal performance | Test Condition | Test Method | ADDIPLAST FRANCE/ADDILENE PMD 50408 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/Af | 66.0 °C |
vicat | ISO 306/A50 | 151 °C | |
Ball pressure temperature | IEC 60335-1 | 140 °C | |
melting temperature | ISO 3146 | 167 °C |