Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PS Stirofor® HI-V0 NATURALE SO.F.TER ITALY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | SO.F.TER ITALY/Stirofor® HI-V0 NATURALE |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 80 J/m |
Electrical performance | Test Condition | Test Method | SO.F.TER ITALY/Stirofor® HI-V0 NATURALE |
---|---|---|---|
Compared to the Leakage Tracking Index (CTI) | IEC 60112 | PLC 2 | |
needle flame test | IEC 60695-11-5 | 通过 |
Mechanical properties | Test Condition | Test Method | SO.F.TER ITALY/Stirofor® HI-V0 NATURALE |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 20 % |
Flexural modulus | ASTM D790 | 2300 MPa | |
tensile strength | 屈服 | ASTM D638 | 30.0 MPa |
flammability | Test Condition | Test Method | SO.F.TER ITALY/Stirofor® HI-V0 NATURALE |
---|---|---|---|
Hot filament ignition temperature | IEC 60695-2-13 | 960 °C | |
UL flame retardant rating | 3.2mm | UL 94 | V-0 |
1.6mm | UL 94 | V-2 | |
Limiting Oxygen Index | ASTM D2863 | 23 % |
physical property | Test Condition | Test Method | SO.F.TER ITALY/Stirofor® HI-V0 NATURALE |
---|---|---|---|
melt mass-flow rate | 200°C/5.0kg | ASTM D1238 | 15 g/10min |
Shrinkage rate | 内部方法 | 0.50 % | |
Water absorption rate | 23°C,24hr | ASTM D570 | 0.060 % |
density | ASTM D792 | 1.17 g/cm³ |
Thermal performance | Test Condition | Test Method | SO.F.TER ITALY/Stirofor® HI-V0 NATURALE |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 77.0 °C |
vicat | ASTM D15253 | 85.0 °C | |
ball-indentation hardness | 75°C | IEC 335 | 通过 |