PPO 100Z-NC ASAHI JAPAN
XYRON™
Fitness equipment、Sports Equipment
Chemical resistance、Low temperature resistanc
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | ASAHI JAPAN/100Z-NC |
---|---|---|---|
Linear thermal expansion coefficient | MD:-30到65°C | ISO11359-2 | 8E-05 cm/cm/°C |
Heat Deflection Temperature | 1.8MPa,未退火 | ASTMD648 | 85.0 °C |
1.8MPa,未退火 | ISO75-2/A | 78.0 °C |
Physical | Test Condition | Test Method | ASAHI JAPAN/100Z-NC |
---|---|---|---|
Modeling Shrinkage | 2.00mm | 内部方法 | 0.50to0.70 % |
Moisture Absorption | 23°C,24hr | ISO62 | 0.10 % |
Mechanical Properties | Test Condition | Test Method | ASAHI JAPAN/100Z-NC |
---|---|---|---|
Nominal Tensile Strain at Break | 23°C | ISO527-2 | 30 % |
Flexural Modulus | 23°C | ISO178 | 2370 Mpa |
Tensile Stress | 屈服,23°C | ISO527-2 | 37.0 Mpa |
Flexural Stress | 23°C | ISO178 | 66.0 Mpa |
Impact Properties | Test Condition | Test Method | ASAHI JAPAN/100Z-NC |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO179 | 16 kJ/m² |
Flammability | Test Condition | Test Method | ASAHI JAPAN/100Z-NC |
---|---|---|---|
Flame Rating | 3.0mm | UL94 | 5VA |
1.5mm | UL94 | V-0 |
Electrical Properties | Test Condition | Test Method | ASAHI JAPAN/100Z-NC |
---|---|---|---|
Dielectric Strength | 2.00mm | IEC60243-1 | 29 KV/mm |
Dielectric Constant | 100Hz | IEC60250 | 2.90 |
Volume Resistivity | 23°C | IEC60093 | 1E+16 ohms·cm |
Surface Resistivity | IEC60093 | 1E+16 ohms | |
Dissipation Factor? | 1MHz | IEC60250 | 4E-03 |
Dielectric Constant | 1MHz | IEC60250 | 2.90 |
Dissipation Factor? | 100Hz | IEC60250 | 3E-03 |