Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
TSU BJB Polyurethane WC-575 A/B BJB Enterprises, Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Supplementary InformationTest ConditionTest MethodBJB Enterprises, Inc./BJB Polyurethane WC-575 A/B
CureTime25°C5.0to7.0 day
hardnessTest ConditionTest MethodBJB Enterprises, Inc./BJB Polyurethane WC-575 A/B
Shore hardness邵氏AASTM D224065to75
thermosettingTest ConditionTest MethodBJB Enterprises, Inc./BJB Polyurethane WC-575 A/B
stripping time25°C5240 min
WorkTime6(25°C)15.0 min
Thermosetting components部件A按重量计算的混合比:100.按容量计算的混合比:100
stripping time25°C4360 min
GelTime25.0 min
Thermosetting mixed viscosity25°C2Brookfield300 cP
Thermosetting components部件B按重量计算的混合比:90.按容量计算的混合比:94
Thermosetting mixed viscosity25°C3Brookfield4730 cP
25°CBrookfield1050 cP
Thermosetting components贮藏期限26 wk
elastomerTest ConditionTest MethodBJB Enterprises, Inc./BJB Polyurethane WC-575 A/B
elongation断裂ASTM D412300 %
tensile strength 断裂ASTM D4129.45 MPa
tear strengthASTM D62411.6 kN/m
physical property Test ConditionTest MethodBJB Enterprises, Inc./BJB Polyurethane WC-575 A/B
Shrinkage rateMDASTM D25660.60 %
density--2ASTM D7921.03 g/cm³
--ASTM D7921.06 g/cm³
--3ASTM D7921.07 g/cm³
特定体积ASTM D7920.947 cm³/g