HDPE PC4012 PEMSB MALAYSIA
--
pipeline
Resistance to stress crac、copolymer
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | PEMSB MALAYSIA/PC4012 |
---|---|---|---|
邵氏D,1秒 | ISO868 | 62 |
Electrical performance | Test Condition | Test Method | PEMSB MALAYSIA/PC4012 |
---|---|---|---|
Volume resistivity | ASTMD257 | 1E+15 ohms·cm | |
dielectric strength | ASTMD149 | 25 KV/mm |
Mechanical properties | Test Condition | Test Method | PEMSB MALAYSIA/PC4012 |
---|---|---|---|
Tensile strain | 断裂 | ISO527-2/2 | 600 % |
Flexural modulus | ISO178 | 850 Mpa | |
Tensile stress | 屈服 | ISO527-2/2 | 23.0 Mpa |
physical property | Test Condition | Test Method | PEMSB MALAYSIA/PC4012 |
---|---|---|---|
melt mass-flow rate | 190°C/2.16kg | ISO1133 | 0.20 g/10min |
Resistance to environmental stress cracking | F0 | ASTMD1693B | 1000 hr |
Thermal performance | Test Condition | Test Method | PEMSB MALAYSIA/PC4012 |
---|---|---|---|
vicat | ISO306/A | 120 °C | |
brittle temperature | ASTMD746 | -100 °C |