| hardness | Test Condition | Test Method | DUPONT USA/SST35 NC010 |
|---|---|---|---|
| Rockwell hardness | R -Sale | ISO 2039-2 | 95 |
| M -Sale | ISO 2039-2 | 50 | |
| injection | Test Condition | Test Method | DUPONT USA/SST35 NC010 |
| Vacuum drying machine | 100 °C | ||
| Temperature in the middle of the barrel | 210 to 215 °C | ||
| desiccant | 除湿 | 80 °C | |
| Temperature at the front of the material cylinder | 215 to 220 °C | ||
| Spray nozzle temperature | 220 to 225 °C | ||
| Mold temperature | 50 to 70 °C | ||
| drying time | 2.0 to 4.0 hr | ||
| Temperature at the rear of the barrel | 175 to 185 °C | ||
| mechanical properties | Test Condition | Test Method | DUPONT USA/SST35 NC010 |
| bending strength | ISO 178 | 76.0 Mpa | |
| Tensile strain | Break | ISO 527-2 | 40 % |
| tensile strength | Break | ISO 527-2 | 46.0 Mpa |
| Bending modulus | ISO 178 | 1800 Mpa | |
| Electrical performance | Test Condition | Test Method | DUPONT USA/SST35 NC010 |
| Volume resistivity | ASTM D257 | 1.0E+13 ohms·cm | |
| Surface resistivity | ASTM D257 | 1.0E+12 ohms | |
| thermal performance | Test Condition | Test Method | DUPONT USA/SST35 NC010 |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 50.0 °C |
| Melting temperature | ISO 11357-3 | 220 °C | |
| Physical properties | Test Condition | Test Method | DUPONT USA/SST35 NC010 |
| Shrinkage rate | Flow | ISO 294-4 | 0.70 - 1.1 % |
| 横向Flow | ISO 294-4 | 0.90 - 1.3 % | |
| water content | < 0.20 % | ||
| flammability | Test Condition | Test Method | DUPONT USA/SST35 NC010 |
| UL flame retardant rating | 3.0 mm | UL 94 | HB |