Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 Alloy INNOMID® CS 6-9000 INNO-COMP HUNGARY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | INNO-COMP HUNGARY/INNOMID® CS 6-9000 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 4.6 kJ/m² |
-30°C | ISO 179/1eA | 3.5 kJ/m² | |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 180 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO 180/A | 4.8 kJ/m² |
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 190 kJ/m² |
Impact strength of cantilever beam gap | -30°C | ISO 180/A | 3.8 kJ/m² |
Mechanical properties | Test Condition | Test Method | INNO-COMP HUNGARY/INNOMID® CS 6-9000 |
---|---|---|---|
Tensile strain | 屈服 | ISO 527-2/1A/50 | 3.6 % |
断裂 | ISO 527-2/1A/50 | 13 % | |
Tensile modulus | ISO 527-2/2 | 3470 MPa | |
Flexural modulus | ISO 178 | 2700 MPa | |
tensile strength | 屈服 | ISO 527-2/1A/50 | 84.0 MPa |
bending strength | ISO 178 | 103 MPa |
Electrical performance | Test Condition | Test Method | INNO-COMP HUNGARY/INNOMID® CS 6-9000 |
---|---|---|---|
Compared to the Leakage Tracking Index (CTI) | 解决方案A | IEC 60112 | PLC 0 |
Volume resistivity | DIN 53482 | 1E+15 ohms·cm |
physical property | Test Condition | Test Method | INNO-COMP HUNGARY/INNOMID® CS 6-9000 |
---|---|---|---|
density | 23°C | ISO 1183 | 1.13 g/cm³ |
Shrinkage rate | TD | ISO 294-4 | 0.80 % |
MD | ISO 294-4 | 0.70 % | |
Melt volume flow rate | 275°C/5.0kg | ISO 1133 | 113 cm³/10min |
Thermal performance | Test Condition | Test Method | INNO-COMP HUNGARY/INNOMID® CS 6-9000 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 175 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 80.0 °C |
Contact Us
Get App
Top