Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Plastomer, Ethylene-based KYOCERA TCG5910 KYOCERA Chemical Corporation
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | KYOCERA Chemical Corporation/KYOCERA TCG5910 |
---|---|---|---|
Shore hardness | 邵氏D,25°C | 80 |
Mechanical properties | Test Condition | Test Method | KYOCERA Chemical Corporation/KYOCERA TCG5910 |
---|---|---|---|
Flexural modulus | 25°C | 3000 MPa |
Electrical performance | Test Condition | Test Method | KYOCERA Chemical Corporation/KYOCERA TCG5910 |
---|---|---|---|
Volume resistivity | 25°C | 1E+15 ohms·cm |
Uncured Properties | Test Condition | Test Method | KYOCERA Chemical Corporation/KYOCERA TCG5910 |
---|---|---|---|
Curing Time | 80°C | 0.50 hr |
Thermal performance | Test Condition | Test Method | KYOCERA Chemical Corporation/KYOCERA TCG5910 |
---|---|---|---|
Glass Transition Temperature | 50.0 °C |