Mechanical properties | Test Condition | Test Method | 3M USA/500GZ |
---|---|---|---|
Tensile strain | 断裂 | ISO 527-1 | 500 % |
Tensile stress | 断裂 | ISO527-2 | 26.0 Mpa |
Flexural modulus | ASTM D790 | 30500 psi | |
ASTMD790 | 210 Mpa | ||
Tensile stress | 断裂 | ISO 527-1 | 3770 psi |
Tensile strain | 断裂 | ISO527-2 | 520 % |
Electrical performance | Test Condition | Test Method | 3M USA/500GZ |
---|---|---|---|
dielectric constant | 23°C,9.40GHz | ASTMD150 | 2.48 |
Dissipation Factor | 1MHz | ASTMD150 | 0.10 |
9.40GHz | ASTMD150 | 0.080 | |
dielectric strength | ASTMD149 | 48 KV/mm | |
dielectric constant | 23°C,1MHz | ASTMD150 | 4.82 |
optical performance | Test Condition | Test Method | 3M USA/500GZ |
---|---|---|---|
refractive index | ASTMD542 | 1.360 | |
transmissivity | 100µm,300nm | 85.0 % | |
100µm,600nm | 93.0 % |
flammability | Test Condition | Test Method | 3M USA/500GZ |
---|---|---|---|
Limiting Oxygen Index | ASTMD2863 | >75 % | |
ASTM D2863 | > 75 % |
physical property | Test Condition | Test Method | 3M USA/500GZ |
---|---|---|---|
melt mass-flow rate | ISO1133 | 10 g/10min | |
ISO 1133 | 10 g/10 min |
Thermal performance | Test Condition | Test Method | 3M USA/500GZ |
---|---|---|---|
melting temperature | ISO12086 | 165 °C | |
ISO 12086 | 329 °F | ||
Glass Transition Temperature | ASTMD4591 | 26.0 °C |