PC GSV-2020R2 MITSUBISHI ENGINEERING JAPAN
IUPILON™ 
Electronic and electrical field
High gloss
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodMITSUBISHI ENGINEERING JAPAN/GSV-2020R2
Hot deformation temperature1.8MPa,Unannealed,6.40mmASTM D648145 °C
Linear coefficient of thermal expansionASTM D6960.000024 cm/cm/℃
UL flame retardant rating1.60mmUL 94V-2
mechanical propertiesTest ConditionTest MethodMITSUBISHI ENGINEERING JAPAN/GSV-2020R2
Bending modulus6.40mmASTM D7906350 Mpa
bending strength6.40mmASTM D790185 Mpa
elongationBreak,3.20mmASTM D6384.0 %
Impact strength of cantilever beam gap3.20mmASTM D256140 J/m
Rockwell hardnessR-SaleASTM D785124
tensile strength3.20mmASTM D638106 Mpa
Electrical performanceTest ConditionTest MethodMITSUBISHI ENGINEERING JAPAN/GSV-2020R2
Dielectric constantASTM D1503.05
Dielectric strengthASTM D14923 KV/mm
Physical propertiesTest ConditionTest MethodMITSUBISHI ENGINEERING JAPAN/GSV-2020R2
melt mass-flow rate300℃/1.2kgASTM D123810-12 g/10min
Shrinkage rateMD:3.00mmASTM D9550.20-0.40 %
Water absorption rate24hrASTM D5700.11 %