TPR GS6000 TEKNOR APEX SINGAPORE
TELCAR®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | TEKNOR APEX SINGAPORE/GS6000 |
---|---|---|---|
邵氏A,10秒 | ASTMD2240 | 60 |
elastomer | Test Condition | Test Method | TEKNOR APEX SINGAPORE/GS6000 |
---|---|---|---|
elongation | 断裂 | ASTMD412 | 650 % |
Tensile stress | 100%应变 | ASTMD412 | 3.00 Mpa |
tensile strength | 屈服 | ASTMD412 | 6.00 Mpa |
Tensile stress | 300%应变 | ASTMD412 | 4.00 Mpa |
physical property | Test Condition | Test Method | TEKNOR APEX SINGAPORE/GS6000 |
---|---|---|---|
melt mass-flow rate | 190°C/2.16kg | ASTMD1238 | 11 g/10min |