Plastic Datasheets

Impact resistanceTest ConditionTest MethodCarmel Olefins Ltd./ TU 75 AV
Impact strength of cantilever beam gap23°CASTM D256450 J/m
23°CISO 18040 kJ/m²
-20°CISO 1809.0 kJ/m²
-20°CASTM D25695 J/m
Mechanical propertiesTest ConditionTest MethodCarmel Olefins Ltd./ TU 75 AV
elongation屈服ASTM D6388.0 %
Flexural modulusASTM D790850 MPa
tensile strength 屈服ASTM D63818.0 MPa
Flexural modulusISO 178850 MPa
Tensile strain屈服ISO 527-2/508.0 %
tensile strength 屈服ISO 527-2/5018.0 MPa
physical property Test ConditionTest MethodCarmel Olefins Ltd./ TU 75 AV
melt mass-flow rate230°C/2.16kgASTM D123835 g/10min
230°C/2.16kgISO 113335 g/10min
Thermal performanceTest ConditionTest MethodCarmel Olefins Ltd./ TU 75 AV
Heat distortion temperature0.45MPa,未退火,HDTASTM D64875.0 °C
vicatASTM D15254140 °C
Heat distortion temperature0.45MPa,未退火,HDTISO 75-2/B70.0 °C
vicatISO 306/A140 °C