| hardness | Test Condition | Test Method | SABIC INNOVATIVE US/3413R-731 |
|---|---|---|---|
| Rockwell hardness | M-Sale | ASTM D785 | 92 |
| R-Sale | ASTM D785 | 120 |
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/3413R-731 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTM D648 | 146 °C |
| 0.45MPa,Unannealed,6.40mm | ASTM D648 | 151 °C | |
| Linear coefficient of thermal expansion | MD:-40to95°C | ASTME831 | 2.2E-05 cm/cm/°C |
| RTI Elec | UL 746 | 120 °C | |
| RTI Imp | UL 746 | 120 °C | |
| RTI Str | UL 746 | 130 °C | |
| specific heat | ASTMC351 | 1130 J/kg/°C | |
| thermal conductivity | ASTMC177 | 0.22 W/m/K | |
| Vicat softening temperature | ASTM D15255 | 165 °C |
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/3413R-731 |
|---|---|---|---|
| Bending modulus | 50.0mmSpan | ASTM D790 | 6610 Mpa |
| bending strength | Yield,50.0mmSpan | ASTM D790 | 153 Mpa |
| elongation | Break | ASTM D638 | 2.0 % |
| Taber abraser | 1000Cycles,1000g,CS-17Wheel | ASTM D1044 | 24.0 mg |
| tensile strength | Break | ASTM D638 | 100 Mpa |
| Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE US/3413R-731 |
|---|---|---|---|
| Arc resistance | ASTM D495 | PLC7 | |
| Compared to the anti leakage trace index | CTI | UL 746 | PLC 5 |
| Dielectric constant | 1MHz | ASTM D150 | 3.31 |
| 50Hz | ASTM D150 | 3.35 | |
| 60Hz | ASTM D150 | 3.35 | |
| Dielectric strength | 3.20mm,inAir | ASTM D149 | 19 KV/mm |
| Dissipation factor | 1MHz | ASTM D150 | 7E-03 |
| 60Hz | ASTM D150 | 1.1E-03 | |
| 50Hz | ASTM D150 | 1.1E-03 | |
| High arc combustion index | HAI | UL 746 | PLC 4 |
| High voltage arc tracing rate | HVTR | UL 746 | PLC 3 |
| Hot wire ignition | HWI | UL 746 | PLC 0 |
| Volume resistivity | ASTM D257 | >1.0E+17 ohms·cm |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/3413R-731 |
|---|---|---|---|
| melt mass-flow rate | 300°C/5.0kg | ASTM D1238 | 19 g/10min |
| 300°C/1.2kg | ASTM D1238 | 5.0 g/10min | |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.10-0.30 % |
| Specific volume | ASTM D792 | 0.697 cm³/g | |
| Water absorption rate | 24hr | ASTM D570 | 0.14 % |
| Equilibrium,23°C | ASTM D570 | 0.26 % |
| impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/3413R-731 |
|---|---|---|---|
| Dart impact | 23°C | ASTM D3029 | 5.00 J |
| Impact strength of cantilever beam gap | ASTM D1822 | 67.0 kJ/m² |
| flammability | Test Condition | Test Method | SABIC INNOVATIVE US/3413R-731 |
|---|---|---|---|
| UL flame retardant rating | 0.75mm | UL 94 | HB |
| 3.0mm | UL 94 | V-0 | |
| 1.5mm | UL 94 | V-1 |