Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PMMA IRK304 MITSUBISHI NANTONG
ACRYPET™
Casters,Automotive components
High temperature resistan,UV resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | MITSUBISHI NANTONG/IRK304 |
---|---|---|---|
Transmittance rate | ASTM D1003 | 92.0 % |
Basic Performance | Test Condition | Test Method | MITSUBISHI NANTONG/IRK304 |
---|---|---|---|
melt mass-flow rate | 230℃37.3N | ASTM D1238 | 3.5 g/10min |
thermal performance | Test Condition | Test Method | MITSUBISHI NANTONG/IRK304 |
---|---|---|---|
Hot deformation temperature | 1.82MPa | ASTM D648 | 94 °C |
Vicat softening temperature | 9.8N | ASTM D1525 | 109 °C |
mechanical properties | Test Condition | Test Method | MITSUBISHI NANTONG/IRK304 |
---|---|---|---|
Bending modulus | ASTM D790 | 2.3 GPa | |
bending strength | ASTM D790 | 78 Mpa | |
Elongation at Break | ASTM D638 | 70 % | |
Impact strength of cantilever beam gap | ASTM D256 | 34 J/m | |
Rockwell hardness | ASTM D785 | 75 M-scale | |
tensile strength | ASTM D638 | 54 Mpa |
Physical properties | Test Condition | Test Method | MITSUBISHI NANTONG/IRK304 |
---|---|---|---|
Shrinkage rate | ASTM D955 | 0.3-0.7 % |