Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA66 DSC221M8 DESCO KOREA
DESLON™ 
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodDESCO KOREA/DSC221M8
Rockwell hardnessR 级ASTM D785120
Mechanical propertiesTest ConditionTest MethodDESCO KOREA/DSC221M8
elongation断裂ASTM D6384.0 %
bending strengthASTM D790127 Mpa
Flexural modulusASTM D7905880 Mpa
tensile strength ASTM D63883.4 Mpa
Electrical performanceTest ConditionTest MethodDESCO KOREA/DSC221M8
Volume resistivityASTM D2571.0E+15 ohms·cm
dielectric strengthASTM D14920 KV/mm
flammabilityTest ConditionTest MethodDESCO KOREA/DSC221M8
UL flame retardant ratingUL 94HB
physical property Test ConditionTest MethodDESCO KOREA/DSC221M8
Water absorption rate24 hr, 23°CASTM D5700.70 %
Shrinkage rateFlow0.60 - 0.80 %
Thermal performanceTest ConditionTest MethodDESCO KOREA/DSC221M8
Heat distortion temperature0.45 MPa, 未退火,HDTASTM D648235 °C
1.8 MPa, 未退火,HDTASTM D648215 °C
melting temperatureDSC260 °C
injectionTest ConditionTest MethodDESCO KOREA/DSC221M8
drying time4.0 to 5.0 hr
Suggested maximum moisture content< 0.20 %
Temperature in the middle of the barrel280 to 285 °C
Temperature at the rear of the barrel270 to 280 °C
Processing (melt) temperature280 to 285 °C
drying temperature80 to 100 °C
Temperature at the front of the material cylinder285 to 290 °C
Temperature80 to 120 °C
Spray nozzle temperature280 to 285 °C