Side track application,Non specific food,Lawn equipment,Garden equipment,Industrial applications,Automotive External Parts,Electrical field,Electronic field,Architectural application field,Outdoor applications,Electrical appliances,Engine hood parts,Medical supplies,Nursing supplies,Plastic bag,Automotive interior parts,Casters
Flame retardant,Glass fiber reinforced
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/DR48-BK1762 |
|---|---|---|---|
| Rockwell hardness | R-Scale | ASTM D785 | 118 |
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/DR48-BK1762 |
|---|---|---|---|
| Ball Pressure Test | 123 to 127°C | IEC 60695-10-2 | 通过 |
| Hot deformation temperature | 0.45 MPa, Unannealed, 6.40 mm | ASTM D648 | 210 °C |
| 1.8 MPa, Unannealed, 6.40 mm | ASTM D648 | 182 °C | |
| Linear coefficient of thermal expansion | 60 to 138°C,Flow | ASTM E831 | 2.0E-5 cm/cm/°C |
| -40 to 40°C,Flow | ASTM E831 | 2.0E-5 cm/cm/°C | |
| RTI | UL 746 | 140 °C | |
| RTI Elec | UL 746 | 120 °C | |
| RTI Imp | UL 746 | 120 °C |
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/DR48-BK1762 |
|---|---|---|---|
| Bending modulus | 50.0 mm Span | ASTM D790 | 5200 Mpa |
| bending strength | Break, 50.0 mm Span | ASTM D790 | 140 Mpa |
| tensile strength | Break | ASTM D638 | 93.0 Mpa |
| Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/DR48-BK1762 |
|---|---|---|---|
| Arc resistance | ASTM D495 | PLC 6 | |
| Compared to the anti leakage trace index | UL 746 | PLC 3 | |
| Dielectric constant | 1 MHz | ASTM D150 | 3.40 |
| 100 Hz | ASTM D150 | 3.60 | |
| Dielectric strength | 1.60 mm, in Oil | ASTM D149 | 25 KV/mm |
| 3.20 mm, in Air | ASTM D149 | 19 KV/mm | |
| Dissipation factor | 1 MHz | ASTM D150 | 0.016 |
| 100 Hz | ASTM D150 | 2.0E-3 | |
| High arc combustion index | UL 746 | PLC 0 | |
| High voltage arc tracing rate | UL 746 | PLC 4 | |
| Hot wire ignition | UL 746 | PLC 3 | |
| Volume resistivity | ASTM D257 | 1.0E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/DR48-BK1762 |
|---|---|---|---|
| Shrinkage rate | Flow : 3.20 to 4.60 mm | Internal Method | 0.60 - 0.90 % |
| Flow : 1.50 to 3.20 mm | Internal Method | 0.40 - 0.60 % | |
| Across FlowFlow : 1.50 to 3.20 mm | Internal Method | 0.50 - 0.80 % | |
| Across FlowFlow : 3.20 to 4.60 mm | Internal Method | 0.80 - 1.1 % | |
| Specific volume | ASTM D792 | 0.650 cm³/g | |
| Water absorption rate | 24 hr | ASTM D570 | 0.070 % |
| impact performance | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/DR48-BK1762 |
|---|---|---|---|
| Suspended wall beam without notch impact strength | 23°C | ASTM D4812 | 500 J/m |
| flammability | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/DR48-BK1762 |
|---|---|---|---|
| Burning wire flammability index | 3.0 mm6 | IEC 60695-2-12 | 960 °C |
| 1.0 mm | IEC 60695-2-12 | 960 °C | |
| Extreme Oxygen Index | ASTM D2863 | 29 % | |
| Hot filament ignition temperature | 3.0 mm | IEC 60695-2-13 | 725 °C |
| 1.0 mm | IEC 60695-2-13 | 700 °C | |
| UL flame retardant rating | 3.0 mm | UL 94 | 5VA |
| 0.9 mm | UL 94 | V-0 |
| injection | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/DR48-BK1762 |
|---|---|---|---|
| Back pressure | 0.300 to 0.700 Mpa | ||
| drying temperature | 120 °C | ||
| drying time | 3.0 to 4.0 hr | ||
| Exhaust hole depth | 0.025 to 0.038 mm | ||
| Mold temperature | 65 to 90 °C | ||
| Processing (melt) temperature | 250 to 265 °C | ||
| Screw speed | 50 to 80 rpm | ||
| Spray nozzle temperature | 245 to 260 °C | ||
| Suggested injection volume | 40 to 80 % | ||
| Suggested maximum moisture content | 0.020 % | ||
| Temperature at the front of the material cylinder | 250 to 265 °C | ||
| Temperature at the rear of the barrel | 240 to 255 °C | ||
| Temperature in the middle of the barrel | 245 to 260 °C |