TPO Advanced Composites ATX832N Advanced Composites, Inc.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Advanced Composites, Inc./Advanced Composites ATX832N |
---|---|---|---|
Dart impact | 0°C | ASTM D3763 | 36.0 J |
Impact strength of cantilever beam gap | 23°C | ISO 180 | 28 kJ/m² |
-40°C | ISO 180 | 5.0 kJ/m² |
hardness | Test Condition | Test Method | Advanced Composites, Inc./Advanced Composites ATX832N |
---|---|---|---|
Shore hardness | 邵氏D,15秒 | ISO 868 | 59 |
Mechanical properties | Test Condition | Test Method | Advanced Composites, Inc./Advanced Composites ATX832N |
---|---|---|---|
tensile strength | 屈服 | ISO 527-2 | 25.0 MPa |
Flexural modulus | ISO 178 | 2180 MPa |
physical property | Test Condition | Test Method | Advanced Composites, Inc./Advanced Composites ATX832N |
---|---|---|---|
melt mass-flow rate | ISO 1133 | 30 g/10min | |
density | ISO 1183 | 1.03 g/cm³ | |
Shrinkage rate | 3.00mm | ISO 294-4 | 9.0E-3-0.011 % |
Thermal performance | Test Condition | Test Method | Advanced Composites, Inc./Advanced Composites ATX832N |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 123 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 64.0 °C |