| machinability | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/LS-2020 9001 |
|---|---|---|---|
| Dry conditions | 热风干燥 120℃---约4-8小时 | ||
| Mold temperature | 70-100 °C | ||
| Screw speed | 50-100 rpm | ||
| Processing temperature | 280-300 °C | ||
| mechanical properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/LS-2020 9001 |
| Tensile modulus | ASTM D638/ISO 527 | 2500 kg/cm²(MPa)[Lb/in²] | |
| Elongation at Break | ASTM D638/ISO 527 | 101 % | |
| Bending modulus | ASTM D790/ISO 178 | 2300 kg/cm²(MPa)[Lb/in²] | |
| bending strength | ASTM D790/ISO 178 | 85 kg/cm²(MPa)[Lb/in²] | |
| Physical properties | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/LS-2020 9001 |
| Shrinkage rate | ASTM D955 | 0.5 - 0.7 % | |
| density | ASTM D792/ISO 1183 | 1.26 | |
| thermal performance | Test Condition | Test Method | MITSUBISHI ENGINEERING JAPAN/LS-2020 9001 |
| Linear coefficient of thermal expansion | ASTM D696/ISO 11359 | 6.6E-05 mm/mm.℃ |