Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 6LVG50H1 BK DOMO CHEM GERMANY
--
Automotive sector,Electronic field,Electrical field
UV resistance,Thermal stability,Glass fiber reinforced
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | DOMO CHEM GERMANY/6LVG50H1 BK |
---|---|---|---|
Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 220 °C |
1.8 MPa, Unannealed | ISO 75-2/A | 210 °C | |
Melting temperature | ISO 11357-3 | 221 °C | |
Vicat softening temperature | ISO 306/B50 | 215 °C |
mechanical properties | Test Condition | Test Method | DOMO CHEM GERMANY/6LVG50H1 BK |
---|---|---|---|
Bending modulus | ISO 178 | 14000 Mpa | |
bending strength | ISO 178 | 320 Mpa | |
Tensile modulus | ISO 527-2/1 | 15500 Mpa | |
Tensile strain | Break | ISO 527-2/5 | 2.0 % |
tensile strength | Break | ISO 527-2/5 | 210 Mpa |
Electrical performance | Test Condition | Test Method | DOMO CHEM GERMANY/6LVG50H1 BK |
---|---|---|---|
Surface resistivity | IEC 60093 | 1.0E+13 ohms | |
Volume resistivity | IEC 60093 | 1.0E+15 ohms·cm |
Physical properties | Test Condition | Test Method | DOMO CHEM GERMANY/6LVG50H1 BK |
---|---|---|---|
Shrinkage rate | 横向Flow : 23°C, 72hr | ISO 2577 | 0.40 - 0.60 % |
Flow : 23°C, 72hr | ISO 2577 | 0.10 - 0.20 % | |
Stickiness | 96% H2SO4 | ISO 307 | 125 cm³/g |
impact performance | Test Condition | Test Method | DOMO CHEM GERMANY/6LVG50H1 BK |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 95 kJ/m² |
Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 90 kJ/m² |
flammability | Test Condition | Test Method | DOMO CHEM GERMANY/6LVG50H1 BK |
---|---|---|---|
Burning rate | FMVSS 302 | < 100 mm/min | |
UL flame retardant rating | 0.8 mm | UL 94 | HB |
injection | Test Condition | Test Method | DOMO CHEM GERMANY/6LVG50H1 BK |
---|---|---|---|
drying temperature | 75 to 85 °C | ||
drying time | 2.0 to 4.0 hr | ||
Mold temperature | 90 to 100 °C | ||
Processing (melt) temperature | 260 to 280 °C |