Ethylene Copolymer Escorene™ Ultra LD 727.22 ExxonMobil
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Test ConditionTest MethodExxonMobil/Escorene™ Ultra LD 727.22
tensile strength 断裂ASTM D6389.74 MPa
Vinyl acetate contentExxonMobilMethod18.0 wt%
Shore hardness邵氏A,15秒ASTM D224092
elongation断裂ASTM D6381500 %
Flexural modulusASTM D79052.7 MPa
melt mass-flow rate190°C/2.16kgASTM D12383.8 g/10min
Shore hardness邵氏D,15秒ASTM D224034
vicatASTM D152559.0 °C