Thermal Properties | Test Condition | Test Method | KURARAY JAPAN/E105A |
---|---|---|---|
Melting temperature (DSC) | ISO 3146 | 165 °C | |
Peak Crystallization Temperature? | DSC | ISO 3146 | 145 °C |
Glass Transition Temperature | DSC | DSC | 53.0 °C |
Physical | Test Condition | Test Method | KURARAY JAPAN/E105A |
---|---|---|---|
Ethylene Content | 44.0 wt% | ||
Melt index | 190℃/2.16 kg | ISO 1133 | 5.7 g/10 min |
210℃/2.16 kg | ISO 1133 | 13 g/10 min |
Mechanical Properties | Test Condition | Test Method | KURARAY JAPAN/E105A |
---|---|---|---|
Tensile Strain | 断裂 | ISO 527-2 | 11 % |
Rockwell Hardness | M 计秤 | ISO 2039-2 | 80 |
Tensile Modulus | ISO 527-2 | 2300 Mpa | |
Charpy Notched Impact Strength | ISO 179 | 2.0 kJ/m² | |
Tensile Stress | 断裂 | ISO 527-2 | 29.0 Mpa |
Flexural Modulus | ISO 178 | 4800 Mpa |