Rubber Techsil® IS803 Techsil Limited
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Techsil Limited/Techsil® IS803 |
|---|---|---|---|
| IRHD hardness | BS903 | 38 |
| Supplementary Information | Test Condition | Test Method | Techsil Limited/Techsil® IS803 |
|---|---|---|---|
| CureTime | 23°C,3.00mm | 7.0 hr | |
| Extrusion rate | 270 g/min | ||
| Young's modulus | 0.700 MPa |
| film | Test Condition | Test Method | Techsil Limited/Techsil® IS803 |
|---|---|---|---|
| Peel strength | 5.3 kN/m |
| thermal performance | Test Condition | Test Method | Techsil Limited/Techsil® IS803 |
|---|---|---|---|
| Linear coefficient of thermal expansion | TD | 9.4E-04 cm/cm/°C | |
| 导热系数 | 0.20 W/m/K | ||
| ServiceTemperature5 | -60-300 °C | ||
| MD | 3.1E-04 cm/cm/°C |
| Electrical performance | Test Condition | Test Method | Techsil Limited/Techsil® IS803 |
|---|---|---|---|
| Dielectric constant | 1MHz | ASTM D150 | 3.00 |
| Dielectric strength | ASTM D149 | 18 kV/mm | |
| Dissipation factor | 1MHz | ASTM D150 | 2.5E-03 |
| Surface resistivity | ASTM D257 | 3.6E+15 ohms | |
| Volume resistivity | ASTM D257 | 1E+16 ohms·cm |
| thermosetting | Test Condition | Test Method | Techsil Limited/Techsil® IS803 |
|---|---|---|---|
| Table drying time | 23°C | 4.0 min |
| Physical properties | Test Condition | Test Method | Techsil Limited/Techsil® IS803 |
|---|---|---|---|
| density | BS903 | 1.07 g/cm³ | |
| Shrinkage rate | MD | <0.80 % |
| elastomer | Test Condition | Test Method | Techsil Limited/Techsil® IS803 |
|---|---|---|---|
| elongation | Break | BS903 | 290 % |
| tear strength | BS903 | 5.50 kN/m | |
| tensile strength | 100%Strain | BS903 | 0.940 MPa |
| Yield | BS903 | 2.30 MPa |