| film | Test Condition | Test Method | EXXONMOBIL SINGAPORE/1002BU |
|---|---|---|---|
| tensile strength | TD : Break | ASTM D882 | 29.0 Mpa |
| Secant modulus -1% secant, TD | ASTM D882 | 220 Mpa | |
| Elmendorf tear strength | MD | ASTM D1922 | 90 g |
| tensile strength | MD : Yield | ASTM D882 | 9.40 Mpa |
| TD : Yield | ASTM D882 | 8.90 Mpa | |
| elongation | TD : Break | ASTM D882 | 800 % |
| tensile strength | MD : Break | ASTM D882 | 49.0 Mpa |
| Elmendorf tear strength | TD | ASTM D1922 | 400 g |
| Dart impact | ASTM D1709A | 70 g | |
| elongation | MD : Break | ASTM D882 | 590 % |
| optical performance | Test Condition | Test Method | EXXONMOBIL SINGAPORE/1002BU |
| turbidity | ASTM D1003 | 4.4 % | |
| gloss | 45° | ASTM D2457 | 76 |
| Physical properties | Test Condition | Test Method | EXXONMOBIL SINGAPORE/1002BU |
| melt mass-flow rate | 190°C/2.16 kg | ASTM D1238 | 2.0 g/10 min |