Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 K-FHG7 DSM HOLAND
Akulon®
--
Glass fiber reinforced,Filler: Glass fiber reinf,35% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | DSM HOLAND/K-FHG7 |
|---|---|---|---|
| Hot deformation temperature | 0.45MPaUnannealed | ISO 75-2/Bf | 220 °C |
| 1.80MPaAnnealed | ISO 75-2/Af | 200 °C | |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 6E-05 cm/cm/°C |
| MD | ISO 11359-2 | 1.5E-05 cm/cm/°C | |
| Vicat softening temperature | Melting Temperature | ISO 11357-3 | 220 °C |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/K-FHG7 |
|---|---|---|---|
| Bending modulus | 23°C | ISO 178 | 10000 Mpa |
| bending strength | 23°C | ISO 178 | 255 Mpa |
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 12 kJ/m² |
| 23°C | ISO 179/1eA | 15 kJ/m² | |
| Elongation at Break | 23°C | ISO 527-2 | 3.30 % |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 70 kJ/m² |
| 23°C | ISO 179/1eU | 95 kJ/m² | |
| Tensile modulus | 23°C | ISO 527-2 | 11000 Mpa |
| tensile strength | 23°C | ISO 527-2 | 185 Mpa |
| flame retardant performance | Test Condition | Test Method | DSM HOLAND/K-FHG7 |
|---|---|---|---|
| UL flame retardant rating | UL -94 | HB 1.50mm |
| Electrical performance | Test Condition | Test Method | DSM HOLAND/K-FHG7 |
|---|---|---|---|
| Dielectric constant | 23°C | IEC 60250 | 3.50 100HZ |
| 23°C | IEC 60250 | 3.30 1MHz | |
| Dissipation factor | 相对漏电起痕指数 | IEC 60112 | 500 V |
| 23°C | IEC 60250 | 0.015 1MHz | |
| 23°C | IEC 60250 | 5E-03 100HZ | |
| Volume resistivity | IEC 60093 | >1.0E+15 Ω.cm |
| Physical properties | Test Condition | Test Method | DSM HOLAND/K-FHG7 |
|---|---|---|---|
| Shrinkage rate | MD | ISO 294-4 | 0.30 % |
| TD | ISO 294-4 | 1.00 % |