Mechanical properties | Test Condition | Test Method | ASCEND USA/50BW |
---|---|---|---|
bending strength | ISO 178 | 33 Mpa | |
tensile strength | 屈服 | ISO 527 | 80 Mpa |
Flexural modulus | ISO 178 | 2900 Mpa | |
Impact strength of simply supported beam without notch | 23℃ | ISO 179 | 6.5 kJ/m² |
elongation | 断裂 | ISO 527 | 45 % |
Impact strength of simply supported beam without notch | -30℃ | ISO 179 | 5.5 kJ/m² |
Tensile modulus | ISO 527 | 3000 Mpa |
Electrical performance | Test Condition | Test Method | ASCEND USA/50BW |
---|---|---|---|
dielectric strength | IEC 60243 | 12 KV/mm | |
Volume resistivity | IEC 60093 | 6 ohm-cm×1015 |
physical property | Test Condition | Test Method | ASCEND USA/50BW |
---|---|---|---|
Shrinkage rate | 2mm,平行 | ISO 294-4 | 1.2 % |
Water absorption rate | 23℃,24hrs | ISO 62 | 1.3 % |
density | ISO 1183 | 1.14 g/cm³ | |
Shrinkage rate | 2mm,垂直 | ISO 294-4 | 1.4 % |
Water absorption rate | 23℃,50%湿度 | ISO 62 | 2.4 % |
Thermal performance | Test Condition | Test Method | ASCEND USA/50BW |
---|---|---|---|
Heat distortion temperature | 0.45MPa,HDT | ISO 75 | 200 °C |
melting temperature | ISO 3146 | 260 °C | |
Heat distortion temperature | 1.82MPa,HDT | ISO 75 | 70 °C |
UL flame retardant rating | UL 94 | V-2 |