Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC/ABS LS-1159 K21441 Samsung Cheil South Korea
INFINO®
Tool handle、TV
Glass fiber reinforced、Flame retardant、Filler: Glass fiber reinf
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Samsung Cheil South Korea/LS-1159 K21441 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 6.0 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 6.0 kJ/m² |
hardness | Test Condition | Test Method | Samsung Cheil South Korea/LS-1159 K21441 |
---|---|---|---|
Rockwell hardness | R级 | ISO 2039-2 | 120 |
R级 | ASTM D785 | 120 |
Mechanical properties | Test Condition | Test Method | Samsung Cheil South Korea/LS-1159 K21441 |
---|---|---|---|
tensile strength | 屈服 | ISO 527-2/5 | 80.0 Mpa |
Tensile modulus | ASTM D638 | 4300 Mpa | |
tensile strength | 断裂 | ISO 527-2/5 | 90.0 Mpa |
elongation | 断裂 | ASTM D638 | 3.3 % |
bending strength | ISO 178 | 110 Mpa | |
ASTM D790 | 120 Mpa | ||
Flexural modulus | ISO 178 | 5000 Mpa | |
Tensile strain | 断裂 | ISO 527-2/5 | 3.3 % |
Tensile modulus | ISO 527-2/5 | 4400 Mpa | |
tensile strength | 断裂 | ASTM D638 | 88.0 Mpa |
屈服 | ASTM D638 | 78.0 Mpa | |
Flexural modulus | ASTM D790 | 4700 Mpa |
flammability | Test Condition | Test Method | Samsung Cheil South Korea/LS-1159 K21441 |
---|---|---|---|
UL flame retardant rating | 2.5mm | UL 94 | V-0 |
3.0mm | UL 94 | V-0 | |
2.0mm | UL 94 | V-0 | |
1.5mm | UL 94 | V-1 |
physical property | Test Condition | Test Method | Samsung Cheil South Korea/LS-1159 K21441 |
---|---|---|---|
melt mass-flow rate | 250°C/2.16kg | ASTM D1238 | 14 g/10min |
250°C/2.16kg | ISO 1133 | 14 g/10min | |
ash content | -- | ASTM D5630 | 15 % |
Shrinkage rate | MD:3.20mm | ASTM D955 | 0.10 % |
TD:3.20mm | ISO 2577 | 0.10 % | |
ash content | -- | ISO 3451 | 15 % |
Shrinkage rate | TD:3.20mm | ASTM D955 | 0.10 % |
MD:3.20mm | ISO 2577 | 0.10 % |
Thermal performance | Test Condition | Test Method | Samsung Cheil South Korea/LS-1159 K21441 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,Unannealed,4.00mm,HDT | ISO 75-2/A | 91.0 °C |
1.8MPa,未退火,6.40mm,HDT | ASTM D648 | 91.0 °C | |
vicat | ISO 306/B50 | 97.0 °C | |
Heat distortion temperature | 0.45MPa,未退火,6.40mm,HDT | ASTM D648 | 96.0 °C |