Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

MABS 950-X02 TORAY JAPAN
--
Electrical applications,OA device,electrical equipment
Detergent resistant,Scratch resistant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | TORAY JAPAN/950-X02 |
---|---|---|---|
Rockwell hardness | R-Sale,23°C | ASTM D785 | 110 |
R-Sale,23°C | ISO 2039-2 | 110 |
thermal performance | Test Condition | Test Method | TORAY JAPAN/950-X02 |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 75.0 °C |
1.8MPa,Unannealed,6.40mm | ASTM D648 | 79.0 °C | |
Vicat softening temperature | 80.0to85.0 °C |
mechanical properties | Test Condition | Test Method | TORAY JAPAN/950-X02 |
---|---|---|---|
Bending modulus | 23°C | ISO 178 | 2180 Mpa |
ASTM D790 | 2100 Mpa | ||
bending strength | 23°C | ISO 178 | 71.0 Mpa |
ASTM D790 | 67.0 Mpa | ||
elongation | Break | ASTM D638 | 20 % |
Tensile strain | Break,23°C | ISO 527-2 | 14 % |
tensile strength | ASTM D638 | 43.0 Mpa | |
Yield,23°C | ISO 527-2 | 50.0 Mpa |
Physical properties | Test Condition | Test Method | TORAY JAPAN/950-X02 |
---|---|---|---|
density | 23°C | ISO 1183 | 1.09 g/cm³ |
ASTM D792 | 1.09 g/cm³ | ||
melt mass-flow rate | 220°C/10.0kg | ISO 1133 | 18 g/10min |
Shrinkage rate | Internal Method | 0.40-0.60 % |
impact performance | Test Condition | Test Method | TORAY JAPAN/950-X02 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 14 kJ/m² |
Impact strength of cantilever beam gap | 23°C,12.7mm | ASTM D256 | 170 J/m |
23°C,3.20mm | ASTM D256 | 180 J/m |
flammability | Test Condition | Test Method | TORAY JAPAN/950-X02 |
---|---|---|---|
UL flame retardant rating | UL 94 | HB |
optical performance | Test Condition | Test Method | TORAY JAPAN/950-X02 |
---|---|---|---|
transmissivity | Total,3000μm | ISO 13468 | 86.0 % |
turbidity | 3000μm | ISO 14782 | 3.0 % |