| mechanical properties | Test Condition | Test Method | DENKA SINGAPORE/MW-1-301 |
|---|---|---|---|
| bending strength | ISO 178 | 102 Mpa | |
| Bending modulus | ISO 178 | 3300 Mpa | |
| Tensile strain | Break | ISO 527-2/5 | <3.0 % |
| tensile strength | Break | ISO 527-2/5 | 47.0 Mpa |
| thermal performance | Test Condition | Test Method | DENKA SINGAPORE/MW-1-301 |
| Vicat softening temperature | ISO 306/B | 93.0 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 74.0 °C |
| optical performance | Test Condition | Test Method | DENKA SINGAPORE/MW-1-301 |
| turbidity | 2000μm | ISO 14782 | 0.30 % |
| transmissivity | 2000μm | ISO 13468 | 90.0 % |
| flammability | Test Condition | Test Method | DENKA SINGAPORE/MW-1-301 |
| UL flame retardant rating | UL 94 | HB | |
| Physical properties | Test Condition | Test Method | DENKA SINGAPORE/MW-1-301 |
| melt mass-flow rate | 200°C/5.0kg | ISO 1133 | 1.8 g/10min |
| hardness | Test Condition | Test Method | DENKA SINGAPORE/MW-1-301 |
| Rockwell hardness | M-Sale,23°C | ISO 2039-2 | 75 |