Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PFA AC-5820 DAIKIN JAPAN
NEOFLON® 
Lining
Weather resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Supplementary InformationTest ConditionTest MethodDAIKIN JAPAN/AC-5820
ContactWater102to106 °
Hexadecane65.0 °
Adhesion Strength PeelTest4.0to6.0 kN/m
hardnessTest ConditionTest MethodDAIKIN JAPAN/AC-5820
Shore hardness邵氏DASTM D224060
Mechanical propertiesTest ConditionTest MethodDAIKIN JAPAN/AC-5820
coefficient of friction与自身-静态内部方法0.050to0.080
Taber abraserCS-17转轮5.00to15.0 mg
tensile strength JISK688819.6to31.4 Mpa
elongation断裂JISK6888250to350 %
physical property Test ConditionTest MethodDAIKIN JAPAN/AC-5820
melt mass-flow rate372°C/5.0kgASTM D33075.0to7.0 g/10min
Particle size150to250 µm
Apparent densityJISK68910.75to1.05 g/cm³
Thermal performanceTest ConditionTest MethodDAIKIN JAPAN/AC-5820
melting temperatureASTM D3307303to313 °C