Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Reference Price
| mechanical properties | Test Condition | Test Method | NATPET SAUDI/HP30G |
|---|---|---|---|
| bending strength | ISO 178 | 85.0 Mpa | |
| Tensile strain | Break | ISO 527-2 | 7.0 % |
| tensile strength | Break | ISO 527-2 | 57.0 Mpa |
| Bending modulus | ISO 178 | 4500 Mpa | |
| injection | Test Condition | Test Method | NATPET SAUDI/HP30G |
| Temperature in the middle of the barrel | 210 to 238 °C | ||
| Temperature at the front of the material cylinder | 204 to 243 °C | ||
| Spray nozzle temperature | 210 to 238 °C | ||
| Mold temperature | 27 to 60 °C | ||
| drying temperature | 71 to 82 °C | ||
| Processing (melt) temperature | 204 to 249 °C | ||
| Temperature at the rear of the barrel | 210 to 238 °C | ||
| Physical properties | Test Condition | Test Method | NATPET SAUDI/HP30G |
| Shrinkage rate | Flow | ISO 294-4 | 0.20 - 0.50 % |
| ash content | ISO 3451-1 | 30 % | |
| melt mass-flow rate | 230°C/2.16 kg | ISO 1133 | 4.5 g/10 min |