Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP PPR PPCO02 Premier Plastic Resins, Inc.
--
--
Filler, glass fiber reinforced material, 20%, filler by weight,
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | Premier Plastic Resins, Inc./PPR PPCO02 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 149 °C |
| 0.45MPa,Unannealed | ASTM D648 | 168 °C |
| mechanical properties | Test Condition | Test Method | Premier Plastic Resins, Inc./PPR PPCO02 |
|---|---|---|---|
| Bending modulus | ASTM D790 | 3100 MPa | |
| elongation | Yield | ASTM D638 | 5.0 % |
| tensile strength | Yield | ASTM D638 | 62.1 MPa |
| Physical properties | Test Condition | Test Method | Premier Plastic Resins, Inc./PPR PPCO02 |
|---|---|---|---|
| density | ASTM D792 | 1.03 g/cm³ | |
| melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 12 g/10min |
| Shrinkage rate | MD | ASTM D955 | 0.60 % |
| impact performance | Test Condition | Test Method | Premier Plastic Resins, Inc./PPR PPCO02 |
|---|---|---|---|
| Impact strength of cantilever beam gap | ASTM D256 | 75 J/m |