plas

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PC H-3000R MITSUBISHI THAILAND
IUPILON™ 
parts,Fitness equipment
High mobility
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

machinabilityTest ConditionTest MethodMITSUBISHI THAILAND/H-3000R
Dry conditions热风干燥 120℃---約4-8小时
Mold temperature70-100 °C
pressure50-150 Mpa
Processing temperature270-290 °C
Screw speed50-100 rpm
thermal performanceTest ConditionTest MethodMITSUBISHI THAILAND/H-3000R
Combustibility (rate)UL 94v2
mechanical propertiesTest ConditionTest MethodMITSUBISHI THAILAND/H-3000R
Charpy Notched Impact StrengthASTM D256/ISO 179NB kg·cm/cm(J/M)ft·lb/in
Elongation at BreakASTM D638/ISO 527118 %
Electrical performanceTest ConditionTest MethodMITSUBISHI THAILAND/H-3000R
Dielectric constantASTM D150/IEC 602503.1
Dielectric lossASTM D150/IEC 602500.0090
Surface resistivityASTM D257/IEC 600936E+15 Ω
Volume resistivityASTM D257/IEC 600933E+14 Ω.cm
otherTest ConditionTest MethodMITSUBISHI THAILAND/H-3000R
characteristic离型改良
ColorN BK
remarksH-3000V(R)
Physical propertiesTest ConditionTest MethodMITSUBISHI THAILAND/H-3000R
densityASTM D792/ISO 11831.20
melt mass-flow rateASTM D1238/ISO 113328 g/10min
Shrinkage rateASTM D9550.50-0.7 %
Water absorption rateASTM D570/ISO 620.24 %