Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

ABS VYTEEN PC/ABS 3016 Lavergne Group
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Lavergne Group/VYTEEN PC/ABS 3016 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 93 J/m |
-29°C | ASTM D256 | 85 J/m | |
Charpy Notched Impact Strength | -30°C | ISO 179/A | 6.0 kJ/m² |
23°C | ISO 179/A | 8.0 kJ/m² |
Mechanical properties | Test Condition | Test Method | Lavergne Group/VYTEEN PC/ABS 3016 |
---|---|---|---|
tensile strength | 屈服2 | ASTM D638 | 80.0 MPa |
bending strength | --3 | ASTM D790 | 140 MPa |
tensile strength | 断裂 | ISO 527-2/5 | 75.0 MPa |
Flexural modulus | --3 | ASTM D790 | 5300 MPa |
--4 | ISO 178 | 5250 MPa | |
bending strength | --4 | ISO 178 | 120 MPa |
flammability | Test Condition | Test Method | Lavergne Group/VYTEEN PC/ABS 3016 |
---|---|---|---|
burning rate | SAEJ369 | 100 mm/min |
physical property | Test Condition | Test Method | Lavergne Group/VYTEEN PC/ABS 3016 |
---|---|---|---|
density | 23°C | ISO 1183 | 1.20 g/cm³ |
ash content | -- | ISO 3451 | 16 % |
density | -- | ASTM D792 | 1.22 g/cm³ |
Shrinkage rate | MD:2.00mm | ASTM D955 | 4.9to6.5 % |
ash content | -- | ASTM D2854 | 16 % |
Shrinkage rate | 3.20mm | ISO 294-4 | 0.30to0.50 % |
Thermal performance | Test Condition | Test Method | Lavergne Group/VYTEEN PC/ABS 3016 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTMD648 | 112 °C |