Material Comparison
Add Comparison Model
Highlight Differences
Hide Same

Product Name / Manufacturer / Model

Brand

Typical Applications

Properties

Color

Form

Processing Methods

Grade

Filler

Recycled Content

Certificates

Reference Price

mechanical propertiesTest ConditionTest MethodKUMHO KOREA/GP-125
Rockwell hardnessASTM D-78574 R scale
bending strength23℃,YieldASTM D-79056.8 Mpa
Bending modulus23℃ASTM D-7902910 Mpa
Impact strength of cantilever beam gap23℃,3.20mmASTM D-25614.9 J/m
Elongation at BreakASTM D-6382.0 %
tensile strengthYieldASTM D-63845.0 Mpa
thermal performanceTest ConditionTest MethodKUMHO KOREA/GP-125
Hot deformation temperature1.80MPa,UnannealedASTM D-64882.0 °C
CombustibilityUL 94HB
Vicat softening temperatureASTM D-152599.0 °C
Physical propertiesTest ConditionTest MethodKUMHO KOREA/GP-125
densityASTM D-7921.04
Shrinkage rateFlowASTM D-9550.30-0.60 %
Basic PerformanceTest ConditionTest MethodKUMHO KOREA/GP-125
Water absorption rateASTM D-5700.030 %
melt mass-flow rate200℃/5kgASTM D-12389.5 g/10min

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China