| flammability | Test Condition | Test Method | DUPONT USA/127UV BK601 |
|---|---|---|---|
| UL flame retardant rating | 0.8mm | UL 94 | HB |
| 0.8mm | IEC 60695-11-10,-20 | HB | |
| FMVSS flammability | FMVSS302 | B | |
| Burning rate | 1.00mm | ISO 3795 | 26 mm/min |
| Fogging-G-value | condensate | ISO 6452 | 1.5E-04 g |
| Supplementary Information | Test Condition | Test Method | DUPONT USA/127UV BK601 |
| EmissionofOrganicCompounds | VDA277 | 16.0 µgC/g | |
| Weather resistance | greyscale | ISO 105-A02 | 42500 |
| Emission | VDA275 | <8.00 mg/kg | |
| Weather resistance | deltaE | DIN 53236 | 0.400 |
| Odor | VDA270 | 3.00 | |
| mechanical properties | Test Condition | Test Method | DUPONT USA/127UV BK601 |
| Nominal tensile fracture strain | ISO 527-2 | 37 % | |
| tensile strength | Yield | ISO 527-2 | 71.5 Mpa |
| Bending modulus | ISO 178 | 2800 Mpa | |
| Tensile modulus | ISO 527-2 | 3000 Mpa | |
| Tensile strain | Yield | ISO 527-2 | 22 % |
| thermal performance | Test Condition | Test Method | DUPONT USA/127UV BK601 |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 162 °C |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1.1E-04 cm/cm/°C |
| MD | ISO 11359-2 | 1.1E-04 cm/cm/°C | |
| AnnealingTemperature | 160 °C | ||
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 92.0 °C |
| Melting temperature | ISO 11357-3 | 178 °C | |
| AnnealingTime-Optional | 30.0 min/mm | ||
| Physical properties | Test Condition | Test Method | DUPONT USA/127UV BK601 |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 2.5 g/10min |