POM 127UV BK601 DUPONT USA
Delrin®
Profile,Plate,Automotive Interior Parts,Automotive sector,Automotive interior parts
Low wear,Photostability,Low volatility
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | DUPONT USA/127UV BK601 |
---|---|---|---|
Emission | VDA275 | <8.00 mg/kg | |
EmissionofOrganicCompounds | VDA277 | 16.0 µgC/g | |
Odor | VDA270 | 3.00 | |
Weather resistance | deltaE | DIN 53236 | 0.400 |
greyscale | ISO 105-A02 | 42500 |
thermal performance | Test Condition | Test Method | DUPONT USA/127UV BK601 |
---|---|---|---|
AnnealingTemperature | 160 °C | ||
AnnealingTime-Optional | 30.0 min/mm | ||
Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 162 °C |
1.8MPa,Unannealed | ISO 75-2/A | 92.0 °C | |
Linear coefficient of thermal expansion | TD | ISO 11359-2 | 1.1E-04 cm/cm/°C |
MD | ISO 11359-2 | 1.1E-04 cm/cm/°C | |
Melting temperature | ISO 11357-3 | 178 °C |
mechanical properties | Test Condition | Test Method | DUPONT USA/127UV BK601 |
---|---|---|---|
Bending modulus | ISO 178 | 2800 Mpa | |
Nominal tensile fracture strain | ISO 527-2 | 37 % | |
Tensile modulus | ISO 527-2 | 3000 Mpa | |
Tensile strain | Yield | ISO 527-2 | 22 % |
tensile strength | Yield | ISO 527-2 | 71.5 Mpa |
Physical properties | Test Condition | Test Method | DUPONT USA/127UV BK601 |
---|---|---|---|
melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 2.5 g/10min |
flammability | Test Condition | Test Method | DUPONT USA/127UV BK601 |
---|---|---|---|
Burning rate | 1.00mm | ISO 3795 | 26 mm/min |
FMVSS flammability | FMVSS302 | B | |
Fogging-G-value | condensate | ISO 6452 | 1.5E-04 g |
UL flame retardant rating | 0.8mm | IEC 60695-11-10,-20 | HB |
0.8mm | UL 94 | HB |