| Basic Performance | Test Condition | Test Method | DSM HOLAND/EM400 |
|---|---|---|---|
| density | ISO 1183 | 1110 kg/m | |
| melt mass-flow rate | ISO 1133 | 30 g/10min | |
| Water absorption rate | ISO 62 | 0.75 % | |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/EM400 |
| tear strength | ISO 34 | 60 kN/m | |
| Tensile modulus | ISO 527 | 50 Mpa | |
| tensile strength | ISO 527 | 25 Mpa | |
| Shore hardness | ISO 868 | 34 - | |
| thermal performance | Test Condition | Test Method | DSM HOLAND/EM400 |
| Vicat softening temperature | ISO 306 | 140 °C | |
| Melting temperature | ISO 11357 | 195 °C | |
| Other performance | Test Condition | Test Method | DSM HOLAND/EM400 |
| Water absorption rate | ISO 62 | 0.3 % |