Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PVOH MonoSol® M8630K MonoSol, LLC
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

filmTest ConditionTest MethodMonoSol, LLC/MonoSol® M8630K
Elmendorf tear strength-MDISO 6383-20.096 N
film thickness38µm.51µm.and76µm
tensile strength --ISO 527-337.2 MPa
Secant modulusASTMD88210.3 MPa
film thickness76 µm
Dart impactASTMD17092200 g
usage76.2µmASTM D43219.96 m²/kg
Elmendorf tear strength-MDASTM D1922940 g
elongation断裂ASTMD882590 %
tensile strength 断裂ASTM D88237.2 MPa
physical property Test ConditionTest MethodMonoSol, LLC/MonoSol® M8630K
solubilityDisintegration:10°C,76.2µm33.0 sec
Dissolution:10°C,76.2µm56.0 sec
water content23°C8.3 wt%

Contact Us

Get App

Top