PPO EXNL1131 BK1066 SABIC INNOVATIVE SHANGHAI
NORYL™
Instrument panel components,Mechanical Engineering,valve
High temperature resistan,Hydrolysis resistance,wear resistant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/EXNL1131 BK1066 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 115 °C |
| 1.8MPa,Unannealed,64.0mmSpan | ISO 75-2/Af | 116 °C | |
| Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 7.4E-05 cm/cm/°C |
| TD:-40to40°C | ISO 11359-2 | 7.4E-05 cm/cm/°C | |
| TD:-40to40°C | ASTME831 | 7.1E-05 cm/cm/°C | |
| MD:-40to40°C | ISO 11359-2 | 7.1E-05 cm/cm/°C | |
| Vicat softening temperature | -- | ISO 306/B120 | 138 °C |
| ASTM D152510 | 136 °C | ||
| -- | ISO 306/B50 | 136 °C |
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/EXNL1131 BK1066 |
|---|---|---|---|
| Bending modulus | 50.0mmSpan | ASTM D790 | 2630 Mpa |
| ISO 178 | 2630 Mpa | ||
| bending strength | Yield,50.0mmSpan | ASTM D790 | 104 Mpa |
| ISO 178 | 107 Mpa | ||
| elongation | Break | ASTM D638 | 29 % |
| Yield | ASTM D638 | 5.2 % | |
| Tensile modulus | ASTM D638 | 2170 Mpa | |
| ISO 527-2/1 | 2910 Mpa | ||
| Tensile strain | Break | ISO 527-2/50 | 21 % |
| Yield | ISO 527-2/50 | 4.9 % | |
| tensile strength | Yield | ASTM D638 | 63.3 Mpa |
| Yield | ISO 527-2/50 | 64.9 Mpa | |
| Break | ISO 527-2/50 | 53.3 Mpa | |
| Break | ASTM D638 | 51.3 Mpa |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/EXNL1131 BK1066 |
|---|---|---|---|
| melt mass-flow rate | 280°C/5.0kg | ASTM D1238 | 9.6 g/10min |
| Melt Volume Flow Rate (MVR) | 280°C/5.0kg | ISO 1133 | 9.85 cm3/10min |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.50-0.80 % |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.050 % |
| Saturation,23°C | ISO 62 | 0.25 % |
| impact performance | Test Condition | Test Method | SABIC INNOVATIVE SHANGHAI/EXNL1131 BK1066 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 16 kJ/m² |
| Dart impact | 23°C,TotalEnergy | ASTM D3763 | 34.2 J |
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 7.8 kJ/m² |
| 23°C | ISO 180/1A | 16 kJ/m² |