Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU CR185A Luborun
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | Luborun/CR185A |
---|---|---|---|
tensile strength | 300%应变 | 9.32 MPa | |
100%应变 | ASTM D-412 | 5.39 MPa | |
tear strength | 断裂 | ASTM D624 | 88.3 kN/m |
compression set | 23℃, 22.0 hr | ASTM D395 | 20 % |
70℃,22.0 hr | 50 | ||
elongation | 断裂 | 800 % | |
tensile strength | 屈服 | 21.6 MPa | |
ASTM D412 | 21.6 MPa | ||
elongation | 断裂 | ASTM D412 | 800 % |
tensile strength | 100%应变 | ASTM D412 | 5.39 MPa |
compression set | 23℃,22.0 hr | ASTM D-395 | 20 % |
tear strength | ASTM D-624 | 88.3 kN/m |
physical property | Test Condition | Test Method | Luborun/CR185A |
---|---|---|---|
density | ASTM D-792 | 1.10 g/cm³ | |
ASTM D-792 | 1.10 g/cm3 | ||
Shore hardness | 支撐 A | ASTM D-2240 | 85 |
支撑A | ASTM D-2240 | 85 |
Thermal performance | Test Condition | Test Method | Luborun/CR185A |
---|---|---|---|
vicat | ASTM D-1525 | 75 ℃ |
Contact Us