EHMWPE Paxon™ AD60-005 ExxonMobil
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Test ConditionTest MethodExxonMobil/Paxon™ AD60-005
tensile strength 屈服ASTM D63832.0 MPa
Flexural modulusASTM D7901480 MPa
Environmental stress cracking resistance100%IgepalASTM D169312.0 hr
densityASTM D48830.963 g/cm³
brittle temperatureASTM D746<-76.0 °C
Impact strength of cantilever beam gapASTM D1822137 kJ/m²
melt mass-flow rate190°C/2.16kgASTM D12380.47 g/10min
vicatASTM D1525127 °C