Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| flammability | Test Condition | Test Method | STYRON TAIWAN/8330 |
|---|---|---|---|
| Hot filament ignition temperature | 2.0mm | IEC 60695-2-13 | 850 °C |
| Burning wire flammability index | 3.0mm | IEC 60695-2-12 | 960 °C |
| UL flame retardant rating | 2.5mm | UL 94 | V-0 |
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 960 °C |
| Hot filament ignition temperature | 3.0mm | IEC 60695-2-13 | 850 °C |
| Burning wire flammability index | 1.0mm | IEC 60695-2-12 | 960 °C |
| Hot filament ignition temperature | 1.0mm | IEC 60695-2-13 | 850 °C |
| mechanical properties | Test Condition | Test Method | STYRON TAIWAN/8330 |
| Tensile modulus | 4.00mm,Injection | ISO 527-2/1 | 2400 Mpa |
| tensile strength | Yield,4.00mm,Injection | ISO 527-2/50 | 60.0 Mpa |
| Break,4.00mm,Injection | ISO 527-2/50 | 58.0 Mpa | |
| Tensile strain | Yield,4.00mm,Injection | ISO 527-2/50 | 6.0 % |
| Break,4.00mm,Injection | ISO 527-2/50 | >100 % | |
| thermal performance | Test Condition | Test Method | STYRON TAIWAN/8330 |
| Vicat softening temperature | ISO 306/A120 | 149 °C | |
| optical performance | Test Condition | Test Method | STYRON TAIWAN/8330 |
| transmissivity | ASTM D1003 | 87.0to91.0 % | |
| Physical properties | Test Condition | Test Method | STYRON TAIWAN/8330 |
| Shrinkage rate | MD | ISO 294-4 | 0.50-0.70 % |
| melt mass-flow rate | 300°C/1.2kg | ISO 1133 | 22 g/10min |